钢板问题

Steel Plate钢板问题

佛山家电彩钢板代客加工配送_为什么pcm彩涂板会掉漆呢?

2021-11-22 10:32| 发布者: steelfu4mo| 查看: 1092| 评论: 0 |原作者: 佛山万庆物资

佛山市万庆物资有限公司10余年的彩钢卷销售过程中,不断的接到客户提到的关于彩钢板的各种各样的问题。当然一些比较复杂的问题是无法用文字来表达的,只能通过电话沟通的方式解决。这也就是常碰到客户发信息问我们的时候,而我们需要问客户电话,打电话给客户的重要原因。

Foshan Wanqing Materials Co., Ltd. In more than 10 years of color steel volume sales process, constantly received customers mentioned about a variety of problems about color steel plate.Of course, some of the more complex problems can not be expressed in words, and can only be solved through telephone communication.That is the important reason why we often encounter a customer to send a message to ask us, and we need to ask the customer phone and call customers.

相信彩涂板的面漆的问题困扰了不少人许久,那为什么总会遇到彩涂板掉漆呢?

Believe that the problem of color paint has troubled many people for a long time, then why always encounter color board paint?

彩涂板的面漆又分为面漆种类、面漆厚度、烘烤时间。面漆种类可分为:普通PE聚酯面漆(一般用)PVDF氟碳树酯面漆(化工用)SMP聚酯面漆(而温,耐磨用)HDP高耐候树酯面漆(海洋气候环境外用)HPC自清洁面漆(粉尘污染用),抗菌聚酯面漆(医疗洁净环境用)

The paint of color coating board is divided into types of paint, paint thickness and baking time.The types of paint can be divided into: general PE polyester paint (general), PVDF fluorocarbon paint (for chemical), SMP polyester paint (while temperature, wear resistant), HDP high resistant tree ester paint (for Marine climate environment), HPC self-cleaning paint (dust pollution), antibacterial polyester paint (for medical clean environment).

除了面漆种类就是面漆厚度了,不管哪种面漆种类,要达到品质要求必须要达到一定的涂膜厚度,大钢厂彩涂板,正面漆一般在18-25um,反面漆一般在8-15um。就像人穿衣服一样,只有把面漆的厚度做足了才能充分抵御外来环境的侵蚀。再一次就是烘烤时间了,当面漆种类很好,面漆膜厚达到,如果烘烤时间不够,面漆就很容易产生粉化和脱落。大钢厂烘箱比小厂一般都要长50-200米。

In addition to the type of paint is paint thickness, no matter which kind of paint, to achieve quality requirements must reach a certain coating thickness, large steel color plate, front paint is generally in 18-25um, reverse paint is generally in 8-15um.Just like people wear clothes, only the thickness of the face paint can fully resist the erosion of the external environment.Once again is the baking time, the face to face paint type is very good, the face paint film thickness is reached, if the baking time is not enough, the face paint is easy to produce powder and fall off.Large steel mill ovens are generally 50-200 meters longer than small factories.

还有就是很多的客户把彩钢卷运到加工厂后,一压制成型就掉漆,或者是把漆面括花,这一般就是压制方式不对,或是钢卷面漆烘烤时间不够,主要原因一般在设备上,有的设备差,滚轮上有很多的毛刺。

There is also a lot of customers after the color steel roll to the processing plant, a suppression molding on the paint, or the paint bracket, this is generally the suppression way is wrong, or the steel coil paint baking time is not enough, the main reason is generally in the equipment, some equipment is poor, there are a lot of burrs on the wheel.

很多工程在彩钢板安装的时候,出现工人不小心用利器划伤面漆,或是在钢板大小不一进行切割的时候,有红热的切割铁屑掉到面漆上,对面漆产生烧灼破坏。彩钢板的面漆本身是一个整体的,如果局部出现划伤,或是烧灼,那就会以点代面的出现红锈,穿孔,最后大面积的生锈漏雨。还有一个不可避免的就是铆钉,铆钉必定会打穿钢板,让彩钢板现现切面,经过雨水流过形成锈蚀。

A lot of projects in the installation of color steel plate installation, workers accidentally scratch the paint with sharp tools, or in the size of the steel plate is different, there are red hot cutting iron chips fell to the paint, the opposite paint produces burning damage.The surface paint of the color steel plate itself is a whole, if the local scratches, or burning, it will replace the surface of red rust, perforation, and finally a large area of rust leakage.There is an inevitable is the rivet, rivevet will break through the steel plate, let the color steel plate now cut, through the rain to form rust.

佛山市万庆物资有限公司作为彩涂板行业的一员,我们一直在孜孜不倦的努力推广彩涂钢板的好处以及高性能彩涂板。佛山万庆公司涂钢板具有良的加工性能,正常使用环境下,漆膜完整性保持10年以上。 

Foshan Wanqing Materials Co., Ltd. As a member of the color coating plate industry, we have been working hard to promote the benefits of color coating steel plate and high-performance color coating steel plate.Foshan Wanqing Company painted steel plate has good processing performance. Under the normal use environment, the integrity of the paint film has been maintained for more than 10 years.

如没特殊注明,文章均为某某科技原创,转载请注明  